《Table 1Textural properties of various supports and the corresponding cata‐lysts.》
本系列图表出处文件名:随高清版一同展现
《合成气直接制烯烃碳化钴基催化剂的载体效应(英文)》
The BET surface area,pore size,and pore volume of the supports and the corresponding supported catalysts are listed in Table 1.The SiO2 support exhibits the highest specific sur‐face area of 459.0 m2/g.The specific surface areas ofγ‐Al2O3and CNT are 184.6 and 170.6 m2/g,respectively.After impreg‐nation,the specific surface area and pore volume decrease dramatically due to the coverage and/or blocking of the pore structure[34].The specific surface areas of Co Mn Na/Si O2,Co Mn Na/γ‐Al2O3,and CoMnNa/CNT decrease to 60.7,72.7,and98.4 m2/g,respectively.The pore volumes of SiO2,γ‐Al2O3,and CNT are 0.78,0.52,and 0.57 cm3/g,respectively.However,the pore volumes of the corresponding catalysts decrease to 0.23,0.21,and 0.37 cm3/g after impregnation,respectively.
图表编号 | XD008200900 严禁用于非法目的 |
---|---|
绘制时间 | 2018.12.01 |
作者 | 王新星、陈文、林铁军、李杰、于飞、安芸蕾、代元元、王慧、钟良枢、孙予罕 |
绘制单位 | 中国科学院上海高等研究院中国科学院低碳转化科学与工程重点实验室、中国科学院大学、中国科学院上海高等研究院中国科学院低碳转化科学与工程重点实验室、中国科学院上海高等研究院中国科学院低碳转化科学与工程重点实验室、中国科学院上海高等研究院中国科学院低碳转化科学与工程重点实验室、中国科学院上海高等研究院中国科学院低碳转化科学与工程重点实验室、中国科学院大学、中国科学院上海高等研究院中国科学院低碳转化科学与工程重点实验室、中国科学院大学、中国科学院上海高等研究院中国科学院低碳转化科学与工程重点实验室、中国科学院大学 |
更多格式 | 高清、无水印(增值服务) |