《Table 3 Fiber lengths of the samples tested using ASTM 519-4 method》
提示:宽带有限、当前游客访问压缩模式
本系列图表出处文件名:随高清版一同展现
《Kenyan Wool Fiber Properties Sampled from Different Sheep Body Parts》
The methods are used depending on the method of sample preparation and how much tension is applied to the individual fibers during preparation and measurement.The results from Table 2 show that SHR samples had the longest fibers w hile BLS samples had the shortest.This is in harmony w ith fact that BLS includes fibers shorn from the legs and the neck area.Also,the CV%w as low est in SHR thus this means that there is less length variation of fibers.The fiber length and other related parameters are given in Table 2 of the samples tested using Almeter.
图表编号 | XD0014953100 严禁用于非法目的 |
---|---|
绘制时间 | 2018.12.31 |
作者 | 王华、MEMON Samiullah、MEMON Hafeezullah |
绘制单位 | College of Textiles,Donghua University、College of Textiles,Donghua University、Donghua University Center for Civil Aviation Composites,Donghua University、Key Laboratory of Textile Science & Technology,Ministry of Education,College of Textiles,Donghua Unive |
更多格式 | 高清、无水印(增值服务) |