《Table 3–The thermal properties of GRS, PVA, CPM and nanofibers obtained from the DSC analyses.》
本系列图表出处文件名:随高清版一同展现
《Preparation of glutinous rice starch/polyvinyl alcohol copolymer electrospun fibers for using as a drug delivery carrier》
The thermal properties of copolymer electrospun fibers of 2%(w/v)GRS with 8%(w/v)PVA that incorporated with 2%(w/v)CPM as model drug revealed three main peaks as shown in Table 3.These peaks corresponded to the approximate peak gelatinization temperature of GRS at 57.33°C,melting temperature of CPM and PVA at 138.31 and 210.25°C,respectively[18,25,30].In the literature,electrospinning has been recognized as the method that can render a drug in its amorphous state because of its extremely fast solvent evaporation resulting in freezing the drug and polymer in a non-equilibrium state[2,9,10,31].The presence of CPM melting peak may cause from the gelatinization analysis method that needs to add some distilled water to the fiber during a DSC experiment.
图表编号 | XD00186265000 严禁用于非法目的 |
---|---|
绘制时间 | 2018.05.01 |
作者 | Patthanakorn Jaiturong、Busaban Sirithunyalug、Sukum Eitsayeam、Chawalinee Asawahame、Pratchaya Tipduangta、Jakkapan Sirithunyalug |
绘制单位 | Department of Pharmaceutical Sciences, Faculty of Pharmacy, Chiang Mai University、Department of Pharmaceutical Sciences, Faculty of Pharmacy, Chiang Mai University、Department of Physics and Materials, Faculty of Science, Chiang Mai University、Department o |