《Table 2 EDS results of as-cast alloys》

《Table 2 EDS results of as-cast alloys》   提示:宽带有限、当前游客访问压缩模式
本系列图表出处文件名:随高清版一同展现
《Effects of Y Content on the Microstructures and Mechanical Properties of Mg-5Zn-xY-0.6Zr Alloys》


  1. 获取 高清版本忘记账户?点击这里登录
  1. 下载图表忘记账户?点击这里登录

Fig.3 shows the SEM images and EDS analysis of as-cast Mg-5Zn-xY-0.6Zr alloys.It illustrates that the reticular intermetallics is made of Mg,Zn and Y in position B.Also the atomic ratio of Y and Zn is nearly 2:3,which is corresponding to the XRD result of W-Mg3Y2Zn3 phase shown in Fig.2.Therefore,the reticular intermetallics phase should be W-Mg3Y2Zn3.Similarly,EDS result of the gray flaked phase in position C is also shown in Table 2.The atomic ratio between Y and Zn is approximately 1:1,which is in accordance with X-Mg12YZn phase shown in Fig.2.Thus,with consideration of the EDS analyses,it can be concluded that WZ505 alloy consists ofα-Mg,W-Mg3Y2Zn3 and X-Mg12YZn phases.WZ805 alloy consists of a-Mg,X-Mg12YZn phase and minor W-Mg3Y2Zn3.Meanwhile,onlyα-Mg and X-Mg12YZn phase exist in WZ1105 alloy.These results are in good agreement with XRD patterns.