《Table 3:EDS results of experimental alloys (wt.%)》

《Table 3:EDS results of experimental alloys (wt.%)》   提示:宽带有限、当前游客访问压缩模式
本系列图表出处文件名:随高清版一同展现
《"Microstructures and tensile properties of as-cast Mg-5Sn-1Si magnesium alloy modified with trace elements of Y, Bi, Sb and Sr"》


  1. 获取 高清版本忘记账户?点击这里登录
  1. 下载图表忘记账户?点击这里登录

Figure 3 shows the XRD results of the modified Mg-5Sn-1Si magnesium alloys.It can be found that after adding 0.8wt.%Y,0.3wt.%Bi,0.9wt.%Sb and 0.9wt.%Sr,respectively,to the Mg-5Sn-1Si alloy,except theα-Mg,Mg2Si,Mg2Sn and Mg2(SixSn1-x) phases,Mg24Y5,Mg3Bi2,Mg3Sb2 and Mg2Sr phases,respectively,were found.The OM images of the modified Mg-5Sn-1Si magnesium alloys are shown in Fig.4 and the corresponding SEM images are shown in Fig.5.The phase compositions measured with EDS are given in Table 3.This indicates that trace elements can not only change the phase morphology but also influence the phase formation in the modified Mg-5Sn-1Si magnesium alloys.