《Table 1 Concrete mix design/ (kg/m3)》
本系列图表出处文件名:随高清版一同展现
《Property and Degradation Characteristics of Concrete Prepared with Aggregate Contained Montmorillonite》
The concrete mix design shown in Table 1 was used.Cement,fly ash and blast furnace slag powder were employed as the binding material.According to Chinese national standard GB 175-2017,cement used in this work pertains to P·O42.5.Fly ash and blast furnace slag powder meet the Chinese national standard GB/T1596-2017 and GB/T 18046-2008,respectively.They belong to Class I and S95 respectively.Cement,fly ash,blast furnace slag powder,fine and coarse aggregates and polycarboxylic acid based water reducing agent were blended with a similar set of parameters as shown in Table 1.The difference was that the coarse aggregate with different contents of montmorillonite was used,C1,C2,C3 and C4 represent respectively the aggregate in which 0,3%,8%,and 16%montmorillonite are appeared.All aggregates meet the requirement for the strength.
图表编号 | XD0043327500 严禁用于非法目的 |
---|---|
绘制时间 | 2019.02.01 |
作者 | 王艳伟、XU Chao、李好新 |
绘制单位 | China Railway No.9 Engineering Testing CO., Ltd、Key Laboratory of Advanced Civil Engineering Materials, Ministry of Education, Tongji University、School of Materials Science and Engineering, Tongji University、Key Laboratory of Advanced Civil Engineering Ma |
更多格式 | 高清、无水印(增值服务) |