《Table 2 Basic parameters of CAC beam》
The coral aggregates natural porous structure,so the part of seawater was pre-absorbed into coral and coral sand.Then the cement,coral aggregate,FA and SG were put into the mixer and mixed for oneminute.Next,the mixture of water-reducer,seawater and inhibitor was added to the mixer,mixing for 3 min.The mixture was poured to shape into CAC beam.After molding,the beam was poured into seawater to cure for 90 d.
图表编号 | XD00180719600 严禁用于非法目的 |
---|---|
绘制时间 | 2020.05.01 |
作者 | 达波、余红发、麻海燕、吴彰钰 |
绘制单位 | Key Laboratory of Coastal Disaster and Defence of Ministry of Education, Hohai University、College of Harbour, Coastal and Offshort Engineering, Hohai University、Department of Civil Engineering, Nanjing University of Aeronautics and Astronautics、Department |