《Table 3 Test results of CAC beam》
Mu of zinc-chromium coated steel(BW8-1)or organic new coated steel(BW6-1)is slightly greater than that of common steel(BW7-2).The main reason is abundant Cl-in the CAC,which leads to severe corrosion of common steel,and narrows the effective section of the steel[18,19],thus reducing the Mu of BW7-2.
图表编号 | XD00180719400 严禁用于非法目的 |
---|---|
绘制时间 | 2020.05.01 |
作者 | 达波、余红发、麻海燕、吴彰钰 |
绘制单位 | Key Laboratory of Coastal Disaster and Defence of Ministry of Education, Hohai University、College of Harbour, Coastal and Offshort Engineering, Hohai University、Department of Civil Engineering, Nanjing University of Aeronautics and Astronautics、Department |
更多格式 | 高清、无水印(增值服务) |