《Table 2 Tensile properties of the joint prepared by SC pin at a given rotational speed of 1000 r/mi
提示:宽带有限、当前游客访问压缩模式
本系列图表出处文件名:随高清版一同展现
《铝锂合金板材摩擦搅拌焊接头组织与力学性能(英文)》
The tensile properties(Table 2)and joint defect(Fig.3)dependence on the welding speed can be explained by the following two factors.The first factor is associated with the metal flow.During the FSW process,the tool rotation opposes the traversing weld direction in the retreating side of the weld.Due to the frictional forces between the tool shoulder and the substrate,the surface material is displaced in both the rotational direction and the welding direction.
图表编号 | XD0011219800 严禁用于非法目的 |
---|---|
绘制时间 | 2018.03.01 |
作者 | 李劲风、陈永来、张绪虎、郑子樵 |
绘制单位 | 中南大学、航天材料及工艺研究所、航天材料及工艺研究所、中南大学 |