《Table 1 Mechanical properties of ACM/AO-80/GO vulcanizates》

《Table 1 Mechanical properties of ACM/AO-80/GO vulcanizates》   提示:宽带有限、当前游客访问压缩模式
本系列图表出处文件名:随高清版一同展现
《Effect of graphene oxide on mechanical properties and damping stability of acrylate rubber/AO-80 composites》


  1. 获取 高清版本忘记账户?点击这里登录
  1. 下载图表忘记账户?点击这里登录

The mechanical properties of ACM/AO-80 vulcanizates filled with different amounts of GO were shown in Table 1,and it was clear that the tensile strength showed an upward trend with the increase of GO amount.The tensile strength and tear strength of ACM/AO-80/GO vulcanizate filled with 1.0 phr GO was 1.72 MPa and 4.57 k N/m,respectively,which increased by 81%and 29.8%compared with those of ACM/AO-80 vulcanizate.It may be due to the formation of effective hydrogen bonds between the oxygen containing functional groups on the GO surface and the carbonyl group in ACM[2].The hydrogen bonds enhanced the compatibility between ACM,AO-80,GO components,which improve the mechanical properties of ACM/AO-80vulcanizate greatly.