《Table 2 EDS analysis of homogenized alloy after 500oC for16 h of point 1 and 2 in Fig.8》

《Table 2 EDS analysis of homogenized alloy after 500oC for16 h of point 1 and 2 in Fig.8》   提示:宽带有限、当前游客访问压缩模式
本系列图表出处文件名:随高清版一同展现
《均匀化处理对Mg-5.9Zn-1.6Zr-1.6Nd-0.9Y合金组织和硬度的影响(英文)》


  1. 获取 高清版本忘记账户?点击这里登录
  1. 下载图表忘记账户?点击这里登录

Microstructure and mechanical properties are changed during homogenization treatment.To some extent,hardness values can confirm the dissolution of constituent particles.In addition,the hardness value is generally used to choose the homogenization process.Therefore,the Vicker’s hardness values of samples homogenized under various condition were tested in this study.For each sample,the average hardness value(HV1)is obtained by randomly selecting 6 points and the variance(σ2)is calculated.These hardness values are presented in Table 3.