《Table 1 Textural properties of MCM-48, Mg-MCM-48-x and Zr-MCM-48-x samples》
![《Table 1 Textural properties of MCM-48, Mg-MCM-48-x and Zr-MCM-48-x samples》](http://bookimg.mtoou.info/tubiao/gif/CPPP201803013_08800.gif)
本系列图表出处文件名:随高清版一同展现
《"Study on Synthesis of Mesoporous M-MCM-48(M=Zr,Mg) and Its Activity for Isomerization of n-Heptane"》
The textural properties of MCM-48,Mg-MCM-48-x(x=0.01,0.02,0.03)and Zr-MCM-48-x(x=0.02,0.04,0.06)are listed in Table 1.In comparison with MCM-48,the specific surface area and pore volume of all samples decreased with an increasing content of incorporated metal(Mg or Zr).This could be probably attributed to the loss of the lattice ordering of MCM-48 framework resulted from the increase in the content of incorporated metal.The degree for loss of the lattice ordering of MCM-48 framework would become greater with an increasing incorporated metal content,and thus the specific surface area and pore volume of the samples could become smaller with the increase in the incorporated metal content.
图表编号 | XD0011306000 严禁用于非法目的 |
---|---|
绘制时间 | 2018.09.30 |
作者 | Wang Yingjun、Dong Xiuli、Ma Shoutao、Wang Jian、Li Xiaoqing、Suo Yanhua、Zhang Wei |
绘制单位 | College of Chemistry and Chemical Engineering, Northeast Petroleum University、College of Chemistry and Chemical Engineering, Northeast Petroleum University、College of Chemistry and Chemical Engineering, Northeast Petroleum University、College of Chemistry |
更多格式 | 高清、无水印(增值服务) |